P. Tucker K. A. Lewis M. P. Hallewell

A typical South Crofty ore containing minor amounts of arsenopyrite and chalcopyrite (ore A) gives 65% overall recovery of cassiterite in the spiral circuit, overall enrichment ratios being about 25-35. Maximum recovery occurs in the size range 53-110 /Lm(Fig. 2). However, recently treated ore types (ore B) have been much richer in sulphides, yielding up to 30°" As in the recleaner table concen...

Journal: :international journal of iron & steel society of iran 2013
j. kamalabadi khorasani a. saeidi a. shafiei

binders are of prime importance in the agglomeration of iron ore concentrates. in this research, strength and density of briquette produced from the magnetite concentrate of gol-e-gohar were investigated using different binders at various applied pressures. the results showed that peridor was the most effective binder relative to bentonite and lime. for all types of binders, the increase in bin...

2016
V. Lishchuk P. Lamberg C. Lund

The main purpose of geometallurgy is to develop a model to predict the variability in the mineral processing performance within the ore body. Geometallurgical tests used for developing such a model need to be fast, practical and inexpensive and include as an input data relevant and measureable geological parameters like elemental grades, mineral grades and grain size. Important in each geometal...

2017
C. Lanzerstorfer

The iron content of the ore used is crucial for the productivity and coke consumption rate in blast furnace pig iron production. Therefore, most iron ore deposits are processed in beneficiation plants to increase the iron content and remove impurities. In several comminution stages, the particle size of the ore is reduced to ensure that the iron oxides are physically liberated from the gangue. ...

Journal: :iranian journal of chemistry and chemical engineering (ijcce) 2007
esmaeil jorjani amir hossein bagherieh bahram rezai

different samples have been prepared from different products in chadormalu iron ore concentrator plant: low intensity magnetite separators concentrate (magnetite concentrate), reverse flotation tail (final hematite concentrate), flotation concentrate (apatite concentrate), final tail (l.i.m.s. tail + reverse flotation concentrate+ apatite flotation tail). the samples were used for rare earth el...

Amir Hossein Bagherieh Bahram Rezai, Esmaeil Jorjani,

Different samples have been prepared from different products in Chadormalu iron ore concentrator plant: Low intensity magnetite separators concentrate (magnetite concentrate), reverse flotation tail (final hematite concentrate), flotation concentrate (apatite concentrate), final tail (L.I.M.S. tail + reverse flotation concentrate+ apatite flotation tail). The samples were used for rare eart...

2011
I. U. Bhuiyan J. Mouzon J. Hedlund S.P.E. Forsmo F. Forsberg

Iron ore concentrate is enriched by flotation prior to form iron ore green pellets in order to reduce phosphorus content in the ore concentrate. A flotation reagent is used in this process and it is known to incorporate air bubbles and eventually deteriorate the strength of the pellets. These bubbles were therefore characterized both qualitatively and quantitatively by cryogenic scanning electr...

ERSHAD-LANGROUDI A., , H. Razavizadeh, ,

A new process for recovering scheelite ores comprises producing a concentrate from the ore, then leaching the concentrate with H_2SO_4 in the presence of H_3PO_4 and Na Cl at atmosphericpressure are discussed. Finely purification of the product will be described. The amounts of dissolution of tungsten in acid depend on the parameters such as time, temperature, type and concentration of acid an...

Journal: :Applied and environmental microbiology 1980
J G Kingma M Silver

Iron-oxidizing thiobacilli were adapted to grow on a chalcopyrite and a galena ore concentrate. When grown on the chalcopyrite concentrate, the bacteria exhibited a doubling time of 38.4 +/- 2.9 h, with a final cellular protein concentration of 185 mug/ml and solubilization of 10.3 g of copper per liter. When grown on the galena ore concentrate, the generation time was 39.6 +/- 2.7 h, with a fi...

2010

Iron ore concentrate sales in a mineral processing plant appeared a trend of high sulfur, exceeding the sales requirement of 0.3% significantly. To this end, for the sulfide in iron concentrate mainly exists in the form of pyrrhotite, companies with iron minerals and has a high degree of oxidation, we can add flotation agent to the magnetic separation column, and at the same time fill gas for s...